Nanoindentation to Microhardness to Tensile Strength Correlation Coefficient Estimates in Relation to Microstructure in Eutectic Snbi Alloy

Nataliya Starostina

Determining strength to hardness correlation coefficients on nano and microscale in correspondence to microstructure and composition leads the way to inexpensive, non-destructive ways to predict tensile strength of bulk materials which is important for developing preventive maintenance procedures in the variety of industries. Nanohardness and microhardness tests were performed on an in-house prepared eutectic SnBi alloy. Elemental composition and eutectic morphology were verified by scanning electron microscopy and energy dispersive spectroscopy. Linear correlation coefficients, C1, between nanoindentation and Vickers microhardness, was determined based on experimental measurements and found to be greater than 1.25. Tabor factor, the ratio of Vickers microhardness to ultimate tensile strength, was estimated to be consistently greater than 3. Comparison to coefficients estimated from data available for other alloy systems is discussed.

免責事項: この要約は人工知能ツールを使用して翻訳されており、まだレビューまたは確認されていません

インデックス付き

Index Copernicus
Open J Gate
Academic Keys
ResearchBible
CiteFactor
Cosmos IF
RefSeek
Hamdard University
Scholarsteer
International Innovative Journal Impact Factor (IIJIF)
International Institute of Organised Research (I2OR)
Cosmos
Geneva Foundation for Medical Education and Research
Secret Search Engine Labs

もっと見る